Polymer Property : Limiting Pressure Velocity = 13500 psi-ft/min
Polymer Property :
Limiting Pressure Velocity =
13500 psi-ft/min
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Limiting Pressure Velocity
0.473
MPa-m/sec
13500
psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet)