Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.54883 MPa-m/sec
15669 psi-ft/min
v = 1m/min
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..