Limiting Pressure Velocity 0.550 MPa-m/sec
15700 psi-ft/min
v = 100m/min
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Limiting Pressure Velocity 0.550 MPa-m/sec
15700 psi-ft/min
LNP EPALP-TB003, at 100 ft/min
Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT)
HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma..