Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.000605 - 0.000654 MPa-m/sec
17.3 - 18.7 psi-ft/min
30 m/min
Polikim EFALON® T-100 Virgin PTFE
Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu..