Polymer Property : Limiting Pressure Velocity = 17500 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF30 TL15 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict..
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF30 TL15 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict..
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF30 TL15 UV 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resist..
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF30 TL15 UV 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resist..
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF30 TL5 LE 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Low Extracta..
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF30 TL5 LE 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Low Extracta..
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF33 TL15 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab..
Limiting Pressure Velocity 0.613 MPa-m/sec
17500 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF33 TL15 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab..