Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.640 MPa-m/sec | 18300 psi-ft/min | |
Kuraray Genestarâ„¢ N1001D-U03 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |