Polymer Property : Limiting Pressure Velocity = 2.80 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0657 - 2.80 MPa-m/sec
1880 - 79900 psi-ft/min
Average value: 1.40 MPa-m/sec Grade Count:10
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..