Mechanical Properties Metric English Comments
Limiting Pressure Velocity 1.05 MPa-m/sec
30000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: ..
Limiting Pressure Velocity 1.05 MPa-m/sec
30000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro..
Limiting Pressure Velocity 1.05 MPa-m/sec
30000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf..
Limiting Pressure Velocity 1.05 MPa-m/sec
30000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance..
Limiting Pressure Velocity 1.05 MPa-m/sec
30000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta..