Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Limiting Pressure Velocity = 31400 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 1.10 MPa-m/sec
31400 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data)
The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also ..
Limiting Pressure Velocity 1.10 MPa-m/sec
31400 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data)
Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C..
Limiting Pressure Velocity 1.10 MPa-m/sec
31400 psi-ft/min
at 0.5 m/s
Shell Carilon® DP P1000 Polyketone  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr..
Limiting Pressure Velocity 1.10 MPa-m/sec
31400 psi-ft/min
Kuraray Genestarâ„¢ N1002A-M41 Nylon
Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel
Limiting Pressure Velocity 1.10 MPa-m/sec
31400 psi-ft/min
Thrust Washer at 0.5 m/s
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it ..