Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.158 MPa-m/sec | 4500 psi-ft/min | 4:1 safety factor applied; QTM 55010 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.158 MPa-m/sec | 4500 psi-ft/min | 4:1 safety factor applied; QTM 55010 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |