Polymer Property : Limiting Pressure Velocity = 51400 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 1.80 MPa-m/sec
51400 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data)
Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic..