Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.200 MPa-m/sec
5710 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data)
Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,..
Limiting Pressure Velocity 0.200 MPa-m/sec
5710 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data)
Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C..
Limiting Pressure Velocity 0.200 MPa-m/sec
5710 psi-ft/min
v = 100m/min
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..