Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Limiting Pressure Velocity = 7140 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.250 MPa-m/sec
7140 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data)
This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica..
Limiting Pressure Velocity 0.250 MPa-m/sec
7140 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Limiting Pressure Velocity 0.250 MPa-m/sec
7140 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data)
FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application..
Limiting Pressure Velocity 0.250 MPa-m/sec
7140 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data)
Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou..
Limiting Pressure Velocity 0.250 - 0.400 MPa-m/sec
7140 - 11400 psi-ft/min
Average value: 0.310 MPa-m/sec Grade Count:4
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Limiting Pressure Velocity 0.250 MPa-m/sec
7140 psi-ft/min
v = 1m/min
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
Copyright © lookpolymers.com All Rights Reserved