Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.330 MPa-m/sec | 9420 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Limiting Pressure Velocity | 0.330 MPa-m/sec | 9420 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo PA 6.6 30% GF Nylon, Glass Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |