Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo RULON® 641 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | |
Saint-Gobain Rulon® 1045 Bearing/Seal PTFE Rulon® 1045 is a dull gold material that has an excellent ability to elongate in a flip seal application. Coupled with excellent frictional characteristics, it offers the added benefit of energy .. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | |
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE Rulon® 1337 is a tan material made entirely from FDA compliant components. It has excellent physical properties and is chemically compatible with most chemicals, except concentrated sulfuric acid.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | |
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for .. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | Max velocity is 2.0 m/s (400 fpm) |
Saint-Gobain Rulon® AR Bearing/Seal PTFE Rulon® AR is somewhat more flexible than Rulon® LR, hence suitable for seals and bonded coating of slide surfaces. It has many decades of use in automotive shaft seals and fuel metering pump c.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | v = 10m/min |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | v = 100m/min |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |