Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 103 MPa | 14900 psi | ASTM D882 |
Solvay Specialty Polymers Ajediumâ„¢ Films -- Polyetherimide Polyether Imide (PEI) Films of polyetherimide (PEI) are amorphous and suitable for high temperature applications. They have an excellent combination of thermal, mechanical and electrical properties, along with very low f.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge Melinex® FRP is designed specifically for embossing and release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and handling properties.Informati.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 103 MPa @Strain 5.00 % |
15000 psi @Strain 5.00 % |
ASTM D882 |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |