Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 1290 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.89 MPa
1290 psi
ASTM D882
NOVA Chemicals Sclair® FG220-A Octene LLDPE Film Resin
Features: Exceptional toughnessLow gel level Applications: Cast stretch wrapNettingCo-extrusion and laminationInformation provided by Nova Chemicals
Film Tensile Strength at Yield, MD 8.90 MPa
1290 psi
ASTM D882
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent..
Film Tensile Strength at Yield, MD 8.90 MPa
1290 psi
ASTM D882
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Film Tensile Strength at Yield, MD 8.90 MPa
1290 psi
ASTM D882
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne..
Copyright © lookpolymers.com All Rights Reserved