Film Tensile Strength at Yield, MD 9.20 MPa
1330 psi
ASTM D 882
NOVA Chemicals Sclair® FP019-C Octene Copolymer LLDPE Film Resin
FP019-C is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Polymer Process AidApplications: High toughness film,..
Film Tensile Strength at Yield, MD 9.20 MPa
1330 psi
ASTM D 882
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin
FP019-D is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Slip, Antiblock, Polymer Process AidApplications: Hig..