Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 12.1 MPa | 1750 psi | |
Dow LDPE 752A Low Density Polyethylene, Film Grade DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu.. |
|||
Film Tensile Strength at Yield, MD | 12.1 MPa | 1750 psi | |
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade DOW LDPE 607A resin is a fully formulated high clarity blown film resin for thin gauge optical applications, such as bakery film. It contains medium levels of slip additive and low levels of antiblo.. |