Polymer Property : Film Tensile Strength at Yield, MD = 1840 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.7 MPa
1840 psi
ASTM D882
LyondellBasell Plexar® PX1007 Extrudable Tie-Layer Resin - Anhydride Modified EVA
ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and ..
Film Tensile Strength at Yield, MD 12.7 MPa
1840 psi
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and..