Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 14.2 MPa
2060 psi
ASTM D 882
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin
FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-..