Polymer Property : Film Tensile Strength at Yield, MD = 22.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 22.8 MPa
3300 psi
ASTM D822
LyondellBasell Alathon® M6020 High Density Polyethylene
ApplicationsALATHON 6020 is a medium molecular high density weight homopolymer for use in blown or cast film applications. This resin provides extremely low gel content and high stiffness. Typica..