Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 21.0 - 35.0 MPa
3050 - 5080 psi
Average value: 28.9 MPa Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..