Film Tensile Strength at Yield, MD 40.7 MPa
5900 psi
ASTM D882
ExxonMobil HDPE HTA 001HD High Density Polyethylene (HMW) Resin
Product Description: HTA 001HD is a high weight HDPE film grade. Films made from HTA 001HD exhibit excellent impact and toughness properties as well as high stiffness. Availability: Africa & Middle ..