Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 42.0 MPa
>= 6090 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, MD >= 42.0 MPa
>= 6090 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, MD 42.0 MPa
6090 psi
ASTM D882
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness...
Film Tensile Strength at Yield, MD 42.0 MPa
6090 psi
ASTM D882
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness...