Polymer Property : Film Tensile Strength at Yield, MD = 7.93 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 7.93 MPa
1150 psi
at 2% offset; ASTM D882
ExxonMobil LL 3002.32 Cast Film Resin  (discontinued **)
LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, ..
Film Tensile Strength at Yield, MD 7.93 MPa
1150 psi
at 2% offset; ASTM D882
ExxonMobil LL 1001.32 Cast Film Resin  (discontinued **)
LL 1001.32 is a butene LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Information provided by ExxonMobil Chemical