Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 8.34 MPa | 1210 psi | at 2% offset; ASTM D882 |
ExxonMobil LL 1237x98 Cast Film Resin
(discontinued **) LL 1237x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 8.34 MPa | 1210 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness.. |