Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 8.55 MPa | 1240 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 2718CB Premium Cast Film Resin Exceed 2718CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 2718CB resin have outstanding tensile properties and impact and puncture toughness.. |