Film Tensile Strength at Yield, MD 8.60 MPa
1250 psi
ASTM D882
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Film Tensile Strength at Yield, MD 8.60 MPa
1250 psi
ASTM D882
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Film Tensile Strength at Yield, MD 8.60 MPa
1250 psi
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Film Tensile Strength at Yield, MD 8.60 MPa
1250 psi
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.