Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.00336 GPa | 0.487 ksi | ASTM D412 Method A |
Seals Eastern 5400 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Secant Modulus | 0.00336 - 0.110 GPa | 0.487 - 16.0 ksi | Average value: 0.0242 GPa Grade Count:52 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |