Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.149 GPa | 21.6 ksi | 0.01; ASTM D638 |
Braskem BI 818 LDPE Injection Molding Polyethylene
(discontinued **) Applications: Injection molding; masterbatches. Information provided by Braskem |
|||
Secant Modulus | 0.149 - 1.45 GPa | 21.6 - 210 ksi | Average value: 0.279 GPa Grade Count:18 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |