Secant Modulus 0.550 GPa
79.8 ksi
1% Secant Modulus; Non-oriented Film; ASTM D882
Total PPR 7450HC Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its ..