Polymer Property : Secant Modulus = 1.374 ksi
Polymer Property :
Secant Modulus =
1.374 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Secant Modulus
0.009473
GPa
1.374
ksi
ASTM D412 Method A
Seals Eastern 5053 Ethylene-Propylene Rubber
General service EPDM.Information provided by Seals Eastern, Inc.