Polymer Property : Secant Modulus = 2.30 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.30 GPa
334 ksi
ASTM D882
DuPont™ Kapton® 100A Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a..
Secant Modulus 2.30 GPa
334 ksi
ASTM D882
DuPont™ Kapton® 200A Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an ar..
Secant Modulus 2.30 GPa
334 ksi
ASTM D882
DuPont™ Kapton® 300A Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a..
Secant Modulus 2.30 GPa
334 ksi
ASTM D882
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an ..