Mechanical Properties Metric English Comments
Secant Modulus 21.72 GPa
3150 ksi
Tensile 0.5% Secant Modulus; ASTM D638
Greene Tweed Arlon® 1263 PEEK, Carbon Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..