Mechanical Properties Metric English Comments
Secant Modulus 0.115 - 0.230 GPa
16.7 - 33.4 ksi
Average value: 0.167 GPa Grade Count:5
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..