Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.3437 GPa | 49.85 ksi | Flexural Secant Modulus; ASTM D6109-97 |
Plastic Lumber from the Plastic Lumber Co. Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep.. |