Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.20 GPa | 754 ksi | ASTM D882 |
DuPont™ Kapton® 200EN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications requ.. |