Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 13 g | 13 g | ASTM D1922 |
Formosa Plastics Formolene® E922 Film HDPE High Density Polyethylene Medium Molecular Weight Bi-Modal Resin Designed for Film Applications Formolene® E922 is a medium molecular weight grade of HDPE designed for good processing characteristi.. |
|||
Elmendorf Tear Strength MD | 13 g | 13 g | ASTM-D1922 |
Braskem FH35 HDPE Cast Film Extrusion Polyethylene Copolymer The FH35 resin is a high-density polyethylene, copolymer of butene-1, produced by the solution process for flat die film extrusion with good mechanical properties. It contains antioxidant additives... |