Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 14 g | 14 g | ASTM D1922 |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |
|||
Elmendorf Tear Strength MD | 14 g | 14 g | ASTM D1922 |
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applicati.. |
|||
Elmendorf Tear Strength MD | 14 g | 14 g | ASTM D1922 |
Formosa Plastics Formolene® E924 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Elmendorf Tear Strength MD | 14 g | 14 g | ASTM D1922 |
Formosa Plastics Formolene® E924F Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Film Applications Formolene® E924F is a “low gel” high molecular weight grade of HDPE designed for high dart impact strength and.. |