Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 10.0 - 250 g
10.0 - 250 g
Average value: 86.8 g Grade Count:10
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..