Polymer Property : Elmendorf Tear Strength MD = 270 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 8.20 - 270 g
8.20 - 270 g
Average value: 96.1 g Grade Count:4
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..