Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 295 g | 295 g | 1 mil; ASTM D1922 |
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial .. |
|||
Elmendorf Tear Strength MD | 295 g | 295 g | ASTM D1922 |
Dow DOWLEX™ 2247G Polyethylene Resin Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap.. |