Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 3.0 g | 3.0 g | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ F15 High Density Polyethylene Film Key Characteristics:High productivityHigh tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierExcellent printabilityRecommended Applications:High speed processingWide l.. |
|||
Elmendorf Tear Strength MD | 3.0 g | 3.0 g | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor.. |
|||
Elmendorf Tear Strength MD | 3.0 g | 3.0 g | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film ( |