Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 380 g
380 g
Eastman D4028-F Polyethylene  (discontinued **)
D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF..
Elmendorf Tear Strength MD 380 g
380 g
Eastman E6838-014F Polyethylene  (discontinued **)
E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta..
Elmendorf Tear Strength MD 380 g
380 g
ASTM D1922
LyondellBasell Petrothene® NA143063 Low Density Polyethylene
ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration..
Elmendorf Tear Strength MD 380 g
380 g
ASTM D1922
ExxonMobil LD 143.26 High Clarity Packaging Film Resin
Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq..
Elmendorf Tear Strength MD 380 g
380 g
ASTM D1922
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin
Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq..
Elmendorf Tear Strength MD 380 g
380 g
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Elmendorf Tear Strength MD 380 g
380 g
ASTM D638
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro..