Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 40.0 - 600 g | 40.0 - 600 g | Average value: 217 g Grade Count:56 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Elmendorf Tear Strength MD | 250 - 600 g | 250 - 600 g | Average value: 465 g Grade Count:10 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Elmendorf Tear Strength MD | 260 - 600 g | 260 - 600 g | Average value: 514 g Grade Count:12 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |