Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 95 g | 95 g | ASTM D1922 |
Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin
(discontinued **) Low Density, Linear Polyethylene Film ResinCustomer Benefits: This unique broad molecular weight distribution resin has a wide processing window and produces film with an excellent combination of to.. |
|||
Elmendorf Tear Strength MD | 95 g | 95 g | ASTM D1922 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |