Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 6.89 MPa | 1000 psi | ASTM D882 |
ExxonMobil LDPE LD 331.08 Low Density Polyethylene Resin Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Availability: Latin Amer.. |
|||
Film Tensile Strength at Break, MD | 6.91 MPa | 1000 psi | ASTM D3759 |
3M Scotch® 3723 High Performance Cold Temperature Box Sealing Tape Scotch® Box Sealing Tape 3723 is a high performance packaging tape for application at refrigeration temperatures, or at room temperature with subsequent storage at low temperatures. This product ha.. |