Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 14.0 - 72.0 MPa
2030 - 10400 psi
Average value: 26.4 MPa Grade Count:257
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..