Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 78.5 MPa | 11400 psi | ASTM D882 |
Lotte Chemical Titan TITANLENE® LDF265YZ Low density polyethylene LDF265YZ is a low density polyethylene resin for film extrusion. LDF265YZ has no slip and anti-block additives. LDF265YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Film Tensile Strength at Break, MD | 78.5 MPa | 11400 psi | ASTM D882 |
Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene HF7000 is a high density polyethylene resin for tubular film extrusion. HF7000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |
|||
Film Tensile Strength at Break, MD | 78.5 MPa | 11400 psi | ASTM D882 |
Lotte Chemical Titan TITANZEX® HF7700 High density polyethylene HF7700 is a high density polyethylene resin for tubular film extrusion. HF7700 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |
|||
Film Tensile Strength at Break, MD | 78.600 MPa | 11400 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil OPPalyte® 278 WOS-2 OPP Film Product Description: One-side treated, on-side sealable, white opaque OPP film with a proprietary cavitated core. WOS-2 was developed to provide improvements over 278 WOS in terms of lower and more .. |